Nozzle 0.4 or 0.6mm Layer 0.08 or 0.12 mm Perimeters 3 Infill 20% Speed External+Small Perimeters 10mm/s Speed Perimeters and Infill 25mm/s
Temp PLA 190-195 (at low speed it should prevent bending of tight corners) Temp PET-G 225-235 ( I have better experience with PET-G not bending so much)